Electron dephasing in homogeneous and inhomogeneous indium tin oxide thin films

arXiv:1202.1627 First posted 2012-02-08 v1 Cited by 22 10 pages, 7 figures
Cite this paper ×
BibTeX
@misc{wu2012electron,
  title = {Electron dephasing in homogeneous and inhomogeneous indium tin oxide thin films},
  author = {Chih-Yuan Wu and Bo-Tsung Lin and Yu-Jie Zhang and Zhi-Qing Li and Juhn-Jong Lin},
  year = {2012},
  eprint = {1202.1627},
  archivePrefix = {arXiv},
  primaryClass = {cond-mat.mes-hall},
  url = {https://arxiv.org/abs/1202.1627}
}
APA
Wu, C.-Y., Lin, B.-T., Zhang, Y.-J., Li, Z.-Q., & Lin, J.-J. (2012). Electron dephasing in homogeneous and inhomogeneous indium tin oxide thin films [Preprint]. arXiv. https://doi.org/10.48550/arXiv.1202.1627
GB/T 7714
WU CY, LIN BT, ZHANG YJ, et al. Electron dephasing in homogeneous and inhomogeneous indium tin oxide thin films[EB/OL]. (2012-02-08)[2026-11-29]. https://arxiv.org/abs/1202.1627.

Abstract

The electron dephasing processes in two-dimensional homogeneous and inhomogeneous indium tin oxide thin films have been investigated in a wide temperature range 0.3-90 K. We found that the small-energy-transfer electron-electron (e-e) scattering process dominated the dephasing from a few K to several tens K. At higher temperatures, a crossover to the large-energy-transfer e-e scattering process was observed. Below about 1-2 K, the dephasing time tau_phi revealed a very weak temperature dependence, which intriguingly scaled approximately with the inverse of the electron diffusion constant D, i.e., tau_phi (T 0.3 rm K) propto 1/D. Theoretical implications of our results are discussed. The reason why the electron-phonon relaxation rate is negligibly weak in this low-carrier-concentration material is presented.