High-pressure optical floating-zone growth of Li(Mn,Fe)PO_4 single crystals

arXiv:1702.01138 First posted 2017-02-03 v1
Cite this paper ×
BibTeX
@misc{neef2017highpressure,
  title = {High-pressure optical floating-zone growth of Li(Mn,Fe)PO_4 single crystals},
  author = {Christoph Neef and Hubert Wadepohl and Hans-Peter Meyer and Rüdiger Klingeler},
  year = {2017},
  eprint = {1702.01138},
  archivePrefix = {arXiv},
  primaryClass = {cond-mat.str-el},
  url = {https://arxiv.org/abs/1702.01138}
}
APA
Neef, C., Wadepohl, H., Meyer, H.-P., & Klingeler, R. (2017). High-pressure optical floating-zone growth of Li(Mn,Fe)PO_4 single crystals [Preprint]. arXiv. https://doi.org/10.48550/arXiv.1702.01138
GB/T 7714
NEEF C, WADEPOHL H, MEYER HP, et al. High-pressure optical floating-zone growth of Li(Mn,Fe)PO_4 single crystals[EB/OL]. (2017-02-03)[2026-11-29]. https://arxiv.org/abs/1702.01138.

Abstract

Mm-sized LiMn_1-xFe_xPO_4 single crystals with 0<= x <= 1 were grown by means of the traveling floating-zone technique at elevated Argon pressure of 30 bar. For the various doping levels, the growth process was optimized with respect to the composition-dependant effective light absorption and transparency of the materials. A convex crystal/melt interface, determined by the angle of incident light, was identified to be particularly crucial for a successful growth. The resulting large single crystalline grains are stoichiometric. Structure refinement shows that lattice parameters as well as the atomic positions and bond lengths linearly depend on the Mn:Fe-ratio. Oriented cuboidal samples with several mm^3 of volume were used for magnetic studies which imply an antiferromagnetic ground state for all compositions. The Néel-temperature changes from T_N = 32.5(5) K in LiMnPO_4 to 49.5(5) K in LiFePO_4 while the easy magnetic axis in the ordered phase flips from the crystallographic a- to the b-axis upon Fe-doping of x<0.2.