Exceeding 400% tunnel magnetoresistance at room temperature in epitaxial Fe/MgO/Fe(001) spin-valve-type magnetic tunnel junctions
@misc{scheike2020exceeding,
title = {Exceeding 400% tunnel magnetoresistance at room temperature in epitaxial Fe/MgO/Fe(001) spin-valve-type magnetic tunnel junctions},
author = {Thomas Scheike and Qingyi Xiang and Zhenchao Wen and Hiroaki Sukegawa and Tadakatsu Ohkubo and Kazuhiro Hono and Seiji Mitani},
year = {2020},
eprint = {2011.08739},
archivePrefix = {arXiv},
primaryClass = {cond-mat.mtrl-sci},
url = {https://arxiv.org/abs/2011.08739}
}
Scheike, T., Xiang, Q., Wen, Z., Sukegawa, H., Ohkubo, T., Hono, K., & Mitani, S. (2020). Exceeding 400% tunnel magnetoresistance at room temperature in epitaxial Fe/MgO/Fe(001) spin-valve-type magnetic tunnel junctions [Preprint]. arXiv. https://doi.org/10.48550/arXiv.2011.08739
SCHEIKE T, XIANG Q, WEN Z, et al. Exceeding 400% tunnel magnetoresistance at room temperature in epitaxial Fe/MgO/Fe(001) spin-valve-type magnetic tunnel junctions[EB/OL]. (2020-11-17)[2026-11-29]. https://arxiv.org/abs/2011.08739.
Abstract
Giant tunnel magnetoresistance (TMR) ratios of 417% at room temperature (RT) and 914% at 3 K were demonstrated in epitaxial Fe/MgO/Fe(001) exchanged-biased spin-valve magnetic tunnel junctions (MTJs) by tuning growth conditions for each layer, combining sputter deposition for the Fe layers, electron-beam evaporation of the MgO barrier, and barrier interface tuning. Clear TMR oscillation as a function of the MgO thickness with a large peak-to-valley difference of 80% was observed when the layers were grown on a highly (001)-oriented Cr buffer layer. Specific features of the observed MTJs are symmetric differential conductance (dI/dV) spectra for the bias polarity and plateau-like deep local minima in dI/dV (parallel configuration) at |V| = 0.2 0.5 V. At 3K, fine structures with two dips emerge in the plateau-like dI/dV, reflecting highly coherent tunneling through the Fe/MgO/Fe. We also observed a 496% TMR ratio at RT by a 2.24-nm-thick-CoFe insertion at the bottom-Fe/MgO interface.