Electroplating of conformal electrodes for vacuum nanogap tunnel junction

Electroplating of conformal electrodes for vacuum nanogap tunnel junction

arXiv:0807.2974 최초 게시 2008-07-18 v3 피인용 4 7 pages, 7 figures, 5 tables
이 논문 인용 ×
BibTeX
@misc{jangidze2008electroplating,
  title = {Electroplating of conformal electrodes for vacuum nanogap tunnel junction},
  author = {Larissa Jangidze and Avto Tavkhelidze and Yujin Blagidze and Zaza Taliashvili},
  year = {2008},
  eprint = {0807.2974},
  archivePrefix = {arXiv},
  primaryClass = {cond-mat.mes-hall},
  url = {https://arxiv.org/abs/0807.2974}
}
APA
Jangidze, L., Tavkhelidze, A., Blagidze, Y., & Taliashvili, Z. (2008). Electroplating of conformal electrodes for vacuum nanogap tunnel junction [Preprint]. arXiv. https://doi.org/10.48550/arXiv.0807.2974
GB/T 7714
JANGIDZE L, TAVKHELIDZE A, BLAGIDZE Y, et al. Electroplating of conformal electrodes for vacuum nanogap tunnel junction[EB/OL]. (2008-07-18)[2026-11-29]. https://arxiv.org/abs/0807.2974.

초록

번역 수정

본 연구에서는 전자 터널링을 위한 대면적 진공 나노갭을 실현하기 위해 Si 기판 위에 Cu 전극을 전기 도금하였다. Cu 전극의 규칙적인 형상을 얻고 내부 장력을 줄이기 위해 음극 코팅, 음극 회전, 비대칭 전류 제도와 전해질 온도 안정화 기법을 사용하였다. 이후 내부 장력을 조절하여 사전 정의된 표면 곡률 (오목 또는 볼록) 을 달성하였다. 12 mm 지름의 Ag/Cu 전극의 경우 Ag 측에서 40 nm/mm 의 곡률을 달성하였으며, 전극 지름을 3 mm 로 줄임으로써 2.5 nm/mm 의 낮은 곡률을 가능하게 하였다. 이는 7 mm² 영역에 걸쳐 5 nm 이하의 나노갭을 갖는 두 개의 접합 전극 제작을 허용한다. 이러한 전극은 혼합 열전자 및 열터널링 영역에서 효율적인 에너지 변환 및 냉각에 활용될 수 있다.